The Development of Unbonded Post-Tensioning Tendons used in Parking Structures in Deicing Salt Regions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Development of Unbonded Post-Tensioning Tendons used in Parking Structures in Deicing Salt Regions

Author(s): C. Walker

Publication: Symposium Paper

Volume: 231

Issue:

Appears on pages(s): 87-104

Keywords: development; parking structures; unbonded

DOI: 10.14359/14922

Date: 10/1/2005

Abstract:
This paper relates the historical development and use of single strandunbonded post-tensioning tendons in parking structures constructed in deicing saltregions in North America since the early 1960’s. These parking structures wereconstructed in southeast Canada and the northeastern and midwestern United Statesusing wire and strand tendons as the primary flexural reinforcing and were exposed todeicing salts during the winter. Parking structures exposed to ocean salts have notbeen reviewed. Most of the following discussion, however, will also apply to them.