Flexural Strengthening of RC Beams Using Steel Reinforced Polymer (SRP) Composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Strengthening of RC Beams Using Steel Reinforced Polymer (SRP) Composites

Author(s): Y.J. Kim, A. Fam, A. Kong, and R. El-Hacha

Publication: Symposium Paper

Volume: 230

Issue:

Appears on pages(s): 1647-1664

Keywords: concrete beam; flexure; Hardwire®; sheet; steel-reinforcedpolymer; strengthening

DOI: 10.14359/14914

Date: 10/1/2005

Abstract:
This paper presents the application of a new generation of externallybonded composite material in flexural strengthening of reinforced concrete beams. Thesteel reinforced polymer (SRP) composite consists of high-carbon steel unidirectionalHardwire® fabrics embedded in epoxy resin, and offers high strength and stiffnesscharacteristics at a reasonable cost. In this paper, the mechanical properties of SRP areevaluated and its application in flexural strengthening of RC beams is investigated. Sixbeams have been tested in three-point bending to study the effect of SRP retrofitting onflexural behavior, failure modes, and crack patterns. Test parameters include variationof the width of SRP sheets and the use of SRP U-wraps to prevent premature failurecaused by delamination of the longitudinal sheet. Significant increase in flexuralcapacity, up to 53%, and pseudo-ductile failure modes were observed in SRP-strengthened beams. Failure was governed primarily by concrete cover delamination atthe ends of SRP sheets or concrete crushing. The U-wraps improved flexural stiffness bymeans of controlling diagonal cracking and providing anchorages to the longitudinalSRP sheets, which reduced their slip. Shear stress concentrations near cut-off points ofSRP sheets have also been investigated. An analytical model was used to predict thenominal flexural strength of SRP-strengthened beams.