Application of Tensioned CFRP Strip Method to an Existing Bridge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Application of Tensioned CFRP Strip Method to an Existing Bridge

Author(s): A. Tateishi, A. Kobayashi, Y. Hamada, T. Takahashi, and H. Yasumori

Publication: Symposium Paper

Volume: 230

Issue:

Appears on pages(s): 1177-1190

Keywords: anchor; prestress; stiffness; strengthening method; tensioned CFRP strip

DOI: 10.14359/14887

Date: 10/1/2005

Abstract:
Tensioned carbon fiber reinforced polymer (CFRP) strip method or Outplate-methodTM was applied to the 28 years old reinforced concrete (RC) box girder bridge inorder to rehabilitate and increase the load capacity of the bridge. The Chofu Bridge hadbeen deteriorated by 28 years of heavy traffic and had many cracks on the underside ofthe main girders. Before and after the CFRP application, on-site load tests of the bridgewere conducted using a 45 ton-weight vehicle. Results of the tensioned CFRP stripapplication to the bridge girders proved effective to reduce the stress in the reinforcingbars and to reduce crack widths.