Finite Element Modelling of RC Beams Retrofitted with CFRP Fabrics

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Finite Element Modelling of RC Beams Retrofitted with CFRP Fabrics

Author(s): H.B. Pham and R. Al-Mahaidi

Publication: Symposium Paper

Volume: 230

Issue:

Appears on pages(s): 499-514

Keywords: CFRP; concrete; debonding; modelling

DOI: 10.14359/14850

Date: 10/1/2005

Abstract:
In this paper, non-linear finite element modelling of debonding failure ofrectangular reinforced-concrete beams strengthened with externally-bonded CarbonFiber Reinforced Polymer (CFRP) fabrics under bending is presented. Smeared crackmodels were used to simulate concrete cracking. Interface elements were used tomodel the bond between concrete and reinforcement. The model proved to be able tosimulate the beams’ behaviour, predicting the failure modes, the failure loads and thereinforcement strain distributions relatively well. The parametric study using the FEAclarified the effect of several important factors on the capacity of the beams.