Analysis of Concrete Placement Load Effects Using Influence Surfaces

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis of Concrete Placement Load Effects Using Influence Surfaces

Author(s): Jui-Lin Peng, David V. Rosowski, Austin D. Pan, Wai-Fah Chen, Siu Lai Chan, and Tsong Yen

Publication: Structural Journal

Volume: 93

Issue: 2

Appears on pages(s): 180-186

Keywords: concrete construction; formwork (construction); influence lines; loads (forces); placing; scaffolds; shoring; Structural Research

DOI: 10.14359/1485

Date: 3/1/1996

Abstract:
A simplified analysis procedure for construction load effects based on the concept of an influence surface is presented. This method can be used to estimate the distribution of shoring loads due to concrete placement and explain the location and magnitude of the maximum shoring load. Since this method is much simpler than performing a complex three-dimensional structural analysis, it has the potential for use by engineers in the design of formwork systems.