Experimental Study of Short NSM–FRP Bar Anchorages

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study of Short NSM–FRP Bar Anchorages

Author(s): D.G. Novidis and S.J. Pantazopoulou

Publication: Symposium Paper

Volume: 230

Issue:

Appears on pages(s): 391-410

Keywords: analytical model; bond; carbon fiber reinforcement polymerbars; mechanical tests; near surface mounted bars; slip

DOI: 10.14359/14844

Date: 10/1/2005

Abstract:
In this paper bond tests conducted on short NSM-bar anchorages arepresented and results are evaluated to determine the effect of design variables ondevelopment capacity. Specimens were designed so as to minimize spurious secondarystresses along the bonded length. Parameters of the study were the groove dimensionsand the embedment length. Bars were CFRP reinforcement with sandblasted surfacecharacteristics. Analytical expressions are derived from first principles so as to interpretthe observed experimental trends. The parameters of the analytical bond stress - slipmodel are calibrated to the experimentally derived bond-slip relationships in order toestablish a limit-state model for post-installed reinforcement, for practical upgradingapplications.