Method for Screening Durability andConstituent Materials in FRP Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Method for Screening Durability andConstituent Materials in FRP Bars

Author(s): D. Gremel, N. Galati, and J. Stull

Publication: Symposium Paper

Volume: 230

Issue:

Appears on pages(s): 153-164

Keywords: alkaline exposure of FRP bars; bending stress; constituentmaterials; durability; GFRP bar

DOI: 10.14359/14830

Date: 10/1/2005

Abstract:
A method for screening the durability of FRP bars under bending stress andimmersion in high pH solution at elevated temperature is described. Discussion of theneed for such a test, process variables affecting durability, determination of theappropriate bending radius and a description of the test method are shown. Testresults from a series of eight production runs varying only one of the processes relatedvariables, glass fiber supplier, are shown. Fiber sizing chemistry for the fiber/resin/production system is key to better durability of GFRP rebar. The bending stressdurability test method helps reveal FRP bar system performance for differentconstituent materials and offers a more practical method for evaluating alkalinedurability of GFRP bars. The method is intended as an indicator of durabilityperformance and not a definitive evaluation.