Tips for Epoxy Resin Injection

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tips for Epoxy Resin Injection

Author(s): John Trout

Publication: Concrete International

Volume: 27

Issue: 11

Appears on pages(s): 44-48

Keywords: repair; epoxy injection; quality control

DOI:

Date: 11/1/2005

Abstract:
Various techniques are presented that will increase the productivity and quality of crack repairs made using epoxy resin injection. Topics ranging from capping techniques to injection pressures to quality control are covered with several photographs explaining the various methods.