Theoretical Model for Confined Steel-Fiber-Reinforced High-Strength Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Theoretical Model for Confined Steel-Fiber-Reinforced High-Strength Concrete

Author(s): H.C. Lima, Jr. and J.S. Giongo

Publication: Symposium Paper

Volume: 229

Issue:

Appears on pages(s): 273-286

Keywords: confinement; high strength concrete; mathematical model; steel fiber

DOI: 10.14359/14742

Date: 9/1/2005

Abstract:
A theoretical model for steel-fiber-reinforced high strength concrete was developed and calibrated against the test results from 86 high-strength concrete columns tested under axial load. The effects of steel-fibers, the concrete compressive strength, and the transverse and longitudinal reinforcement ratio were accounted for in the proposed stress-strain model. The current model is based on the model developed by Cusson and Paultre, in which the effect of steel-fibers on the concrete ductility was incorporated using the reinforcement index of the volumetric ratio of the steel-fiber addition. The agreement between the model responses and test results was satisfactory.