Self Consolidating Concrete, High-Performance and Normal Concrete Affected by Creep at Different Age, Curing, Load Level, Strength, and Water-Cement Ratio with some Interrelated Properties

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Self Consolidating Concrete, High-Performance and Normal Concrete Affected by Creep at Different Age, Curing, Load Level, Strength, and Water-Cement Ratio with some Interrelated Properties

Author(s): B. Persson

Publication: Symposium Paper

Volume: 229

Issue:

Appears on pages(s): 63-92

Keywords: autogenous shrinkage; basic creep; creep; creep coefficient; elastic modulus; moisture; relative humidity; shrinkage

DOI: 10.14359/14729

Date: 9/1/2005

Abstract:
This article outlines an extensive number of laboratory tests on long-term deformations of Self Consolidating Concrete, SCC. For this purpose 4 SCC and 4 vibrated concrete, VC, were fabricated, in all 88 creep specimens. The water-cement ratio, w/c, of the concrete varied between 0.27 and 0.80 and strength between 14 and 171 MPa. Studies on shrinkage, strength and relative humidity, RH, were performed in parallel. The effect of late start of drying on creep was also incorporated in the studies. The results show creep and shrinkage of SCC of the same range of order as for VC at constant strength. No significant difference between the elastic modulus of SCC and that of VC was observed at constant strength. The creep coefficient , o, developed similarly in SCC as in VC .