Discussion from the November-December 2004 ACI Structural Journal/Page 755 (101-S74)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Discussion from the November-December 2004 ACI Structural Journal/Page 755 (101-S74)

Author(s): Emil de Souza Sanchez Filho, Marta de Souza Lima Velasco, and Ricardo Amorim Einsfeld

Publication: Structural Journal

Volume: 102

Issue: 5

Appears on pages(s): 784-785

Keywords:

DOI: 10.14359/14674

Date: 9/1/2005

Abstract:
Disc. 101-S74/From the November-December 2004 ACI Structural Journal, p. 755 Analytical Model to Evaluate Failure Behavior of Plated Reinforced Concrete Beams Strengthened for Shear. Paper by Vincenzo Colotti, Giuseppe Spadea, and R. Narayan Swamy


ALSO AVAILABLE IN:

Electronic Structural Journal