Concrete Durability

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Durability

Author(s): Neal S. Berke, Maria C. Hicks, James Malone, and Klaus A. Rieder

Publication: Concrete International

Volume: 27

Issue: 8

Appears on pages(s): 63-68

Keywords: corrosion; corrosion rate; permeability; corrosion inhibitor; life-cycle cost; shrinkage reducing admixture

DOI:

Date: 8/1/2005

Abstract:
For concretes used in applications with high levels of chloride exposure, special systems can be specified to increase concrete durability. These systems work by reducing the rate of ingress of chloride, increasing the chloride level at which corrosion initiates, or reducing the rate of corrosion at active corrosion cells. Once the performance of the available corrosion protection systems is quantified, computer models can be used to perform life-cycle cost analyses for selection the most cost-effective combinations. An example analysis is provided.