From Research to Better Practice

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: From Research to Better Practice

Author(s): Francois Toutlemonde

Publication: Concrete International

Volume: 27

Issue: 8

Appears on pages(s): 49-53

Keywords: concrete durability; high performance concrete; nanoscience; preservation; rheology

DOI:

Date: 8/1/2005

Abstract:
The “Architecture and Concrete” conference, held on December 6-7, 2004, in Paris, France, was the final international event in ACI’s Centennial year. Part of this conference was a session devoted to exploring how research has led to better practice in the field of concrete. This article provides a summary of the major points of the sessions that covered topics such as durability, preservation, rheology, nanoscience, and new concretes.