Acoustic Emission Response and Mechanical Characterization of Ultra High-Performance Concrete Types

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Acoustic Emission Response and Mechanical Characterization of Ultra High-Performance Concrete Types

Author(s): S. Marijan, B. Dubravka, and S. Zeljana

Publication: Symposium Paper

Volume: 228

Issue:

Appears on pages(s): 1207-1220

Keywords: acoustic emission; high-performance fibre reinforcedconcrete; toughness

DOI: 10.14359/14532

Date: 6/1/2005

Abstract:
Construction of modern structures and reconstruction of the existing onesimpose very demanding requirements for the quality of used materials. Highperformance hybrid fibre reinforced concrete appears to be a material of great importance in the future. An innovative type of this concrete was tested and its properties were compared with those of reactive powder concrete, high performanceconcrete and plain concrete. Compressive strength, flexural strength, toughness and modulus of elasticity were measured. For the purposes of toughness testing, an acousticemission technique was used to detect cracking and fracture properties.