Development and Construction Record on High-Strength Concrete with the Compressive Strength Exceeding 150 Mpa

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development and Construction Record on High-Strength Concrete with the Compressive Strength Exceeding 150 Mpa

Author(s): H. Jinnai, S. Kuroiwa, S. Watanabe, S. Namiki, and M. Hayakawa

Publication: Symposium Paper

Volume: 228

Issue:

Appears on pages(s): 1045-1062

Keywords: 150MPa; construction record; high-strength concrete; mock-up; unit water content

DOI: 10.14359/14520

Date: 6/1/2005

Abstract:
In this study, concretes with a compressive strength exceeding 150 MPa were produced using mixers at a ready-mixed concrete plant. Tests were conducted on the production method and workability of these concretes and their strength development in mock-up columns, in winter and summer. Based on the results of these tests, concretes with a compressive strength exceeding 150 MPa were used for the construction of a high-rise building. Concretes with a compressive strength exceeding 150 MPa were produced using a binder comprised of ordinary portland cement, slag gypsum and silica fume. The results of quality control tests for unit water content, slump flow, air content and compressive strength showed that concretes with compressive strength exceeding 150 MPa were produced and placed to a consistent quality.