Bond Anchorgae Behavior of Pretensioned Tendons in High-Performance Concrete (HPC)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bond Anchorgae Behavior of Pretensioned Tendons in High-Performance Concrete (HPC)

Author(s): J. Hegger, B. Kommer, S. Bulte, and A. Sherif

Publication: Symposium Paper

Volume: 228

Issue:

Appears on pages(s): 495-512

Keywords: anchorage; bond; concrete cover; high-performanceconcrete; pull-out tests; transmission length

DOI: 10.14359/14488

Date: 6/1/2005

Abstract:
Numerous pull-out tests, tests on the transfer of prestressing forces, and load bearing tests on pretensioned beams made of High Performance Concrete (HPC) have been conducted. Using these tests the bond properties of 7-wire strands (dp = 0.5 in. = 12.5 mm) and ribbed wires Ø 12 mm are investigated. The lateral strain-dependent bond behavior in different types of concrete as well as the general transfer of prestressing forces are determined. Hereby, missing bases for code specifications, regulations and standards are derived for the use of bond anchorages of pretensioned tendons. The corresponding test results are presented and compared with current code specifications from Europe and the US. Furthermore, initial test results are presented concerning the influence of lateral tension and longitudinal cracks in the surrounding concrete on the anchorage of pretensioned strands.