Title: The Tolerance Cloud

Author(s): Dick Birley

Publication: Concrete International

Volume: 27

Issue: 6

Appears on pages(s): 61-63

Keywords: reinforcing; tolerance; constructibility

DOI:

Date: 6/1/2005

Abstract:
This article is the first in a series to be contributed by members of ACI Committee 315-B, Details of Concrete Reinforcement-Constructability. The series will examine reinforcing steel constructability issues commonly encountered in the field. Solutions to these issues that are based on actual job-site experience will be presented. This first article discusses the fabrication tolerances for a simple bar with 90 degree hooks at each end.