Composite Moment Frames

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Composite Moment Frames

Author(s): Gregory G. Deierlein, Paul Cordova, Keh-Chyuan Tsai, Chui-Hsin Chen, and Wen-Chi Lai

Publication: Concrete International

Volume: 27

Issue: 5

Appears on pages(s): 39-44

Keywords: composite moment frames; full-scale frame testing; beam-column design; precast construction; seismic performance

DOI:

Date: 5/1/2005

Abstract:
Studies have demonstrated that composite systems have the strength, stiffness, and ductility to safely resist large earthquakes. This recent full-scale frame test further validates the reliability of the composite frames using innovative precast construction details. Designed to just meet the minimum requirements of current building code standards, the test frame performed very well under three earthquake loading scenarios and a final pushover test. Overall, the test frame clearly demonstrates the capabilities of composite moment frames to meet and exceed the seismic performance expectations implied by modern building codes.