New Code Provisions for Long Term Deflection Calculations

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: New Code Provisions for Long Term Deflection Calculations

Author(s): R. H. Scott and A. W. Beeby

Publication: Symposium Paper

Volume: 225

Issue:

Appears on pages(s): 119-132

Keywords: codes and standards; deflection control; structural concrete

DOI: 10.14359/14380

Date: 3/1/2005

Abstract:
Current code provisions for deflection calculations in reinforced concrete beams and slabs are discussed. A comprehensive series of laboratory tests to investigate long term tension stiffening effects is summarised, results from which indicated that tension stiffening decays much more rapidly than was previously understood. Revised code provisions are proposed based on this finding.