Title: Fiber Composite Sheets in Cold Climate Rehab

Author(s): Kenneth W. Neale and Pierre Labossiere

Publication: Concrete International

Volume: 20

Issue: 6

Appears on pages(s): 22-24

Keywords: composite materials; environments; repairs; strengthening

DOI:

Date: 6/1/1998

Abstract:
The main focus of this paper is recent field applications of composite repair techniques in the Canadian province of Quebec. This region of North America is subjected to harsh winter climates. To assess the viability of composite wrapping technology in such severe environments, a number of field applications have recently been undertaken in conjunction with research at the University of Sherbrooke, Quebec.