PCP: Pervious Concrete Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: PCP: Pervious Concrete Pavements

Author(s): Portland Cement Association

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 36

Keywords:

DOI:

Date: 2/1/2005

Abstract:
Pervious concrete as a paving material has seen renewed interest due to its ability to allow water to flow through itself to recharge groundwater and minimize stormwater runoff. This introduction to pervious concrete pavements reviews its applications and engineering properties, including environmental benefits, structural properties, and durability. Both hydraulic and structural design of pervious concrete pavements are discussed, as well as construction techniques.