355.2-04/355.2R-04: Qualification of Post-Installed Mechanical Anchors in Concrete and Commentary

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 355.2-04/355.2R-04: Qualification of Post-Installed Mechanical Anchors in Concrete and Commentary

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 31

Keywords: anchors; cracked concrete; expansion anchors; fasteners; mechanical anchors; post-installed anchors; undercut anchors.

DOI:

Date: 10/27/2004

Abstract:

Note: A newer version of this document exists. This document was replaced by 355.2-07.

ACI 355.2 prescribes testing programs and evaluation requirements for post-installed mechanical anchors intended for use in concrete under the design provisions of ACI 318. Criteria are prescribed for determining whether anchors are acceptable for use in uncracked concrete only, or in cracked as well as uncracked concrete. Performance categories for anchors are established, as are the criteria for assigning anchors to each category. The anchor performance categories are used by ACI 318 to assign capacity reduction factors and other design parameters.