Repairing and Retrofitting Post-Tensioned Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Repairing and Retrofitting Post-Tensioned Beams

Author(s): P. R. Chakrabarti

Publication: Concrete International

Volume: 27

Issue: 2

Appears on pages(s): 45-48

Keywords: fiber-reinforced polymer; E-glass; carbon fiber

DOI:

Date: 2/1/2005

Abstract:
Traditionally, unbonded, prestressed concrete structures are repaired by one of two methods: replacing the old tendons r adding new tendons and a new layer of concrete. Fiber-reinforced polymer (FRP) and adhesives promised an alternate repair solution. The information presented in this article is the result of a research project performed to understand the behavior of prestressed, post-tensioned beams that are repaired or retrofit with FRP.