Title: SP-194: The Adam Neville Symposium: Creep and Shrinkage-Structural Design Effects

Author(s): Editor: Akthem Al-Manaseer / Sponsored by: ACI Committee 209

Publication: Symposium Paper

Volume: 194

Issue:

Appears on pages(s): 424

Keywords:

DOI: 10.14359/14228

Date: 5/1/2000

Abstract:
This Symposium Publication contains 12 papers presented at the Adam Neville Symposium in Atlanta, Georgia, in 1997. Topics relating to creep and shrinkage include admixture and cementitious materials effects, special high-performance considerations, temperature and humidity influences, reinforced and prestressed concrete analysis and design procedures, and much more. Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP194