Title: SP-182: Structural Applications of Fiber Reinforced Concrete

Author(s): Editors: N. Banthia, C. MacDonald, and P. Tatnall

Publication: Symposium Paper

Volume: 182

Issue:

Appears on pages(s): 257

Keywords:

DOI: 10.14359/14175

Date: 5/1/1999

Abstract:
This Symposium Publication presents 13 papers on the use of fiber reinforcement in structural applications and assembles the thoughts of some leading researchers in the field. Collectively, these writings are a snapshot of contemporary thinking in this field and provide a direction for future activity. Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP182