Title: SP-122: Paul Klieger Symposium on Performance of Concrete

Author(s): Editor: David Whiting / Co-Sponsored by: ACI Committees 201 and ACI Committee 222

Publication: Symposium Paper

Volume: 122

Issue:

Appears on pages(s): 499

Keywords:

DOI: 10.14359/14155

Date: 6/1/1990

Abstract:
"A collection of 24 papers form an international panel of experts on topics ranging from fundamental laboratory studies of concrete durability to case histories of concrete rehabilitation. The volume is arranged in three parts. Part 1: covers the more fundamental aspects and laboratory investigations. Topics include freeze-thaw resistance, durability of high strength concrete, corrosion of reinforcing steel, air voids in concrete, and effects of high range water-reducers. Part 2: covers field studies where concrete is exposed to natural conditions. Topics include carbonation of concrete, deicer scaling resistance of roller compacted concrete pavements, performance in marine environments, and microbiologically-induced deterioration. Part 3: covers case histories of the performance and rehabilitation of concrete structures in severe service environments. The types of structures include cooling tower shells, precast prestressed concrete conveyor bridge, heavy duty dock, elevated road way, and a masonry structure under corrosive exposure." Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP122