Title: SP-121: High-Strength Concrete: Second International Symposium

Author(s): Weston T. Hester

Publication: Symposium Paper

Volume: 121

Issue:

Appears on pages(s): 786

Keywords:

DOI: 10.14359/14154

Date: 11/1/1990

Abstract:
SP-121 The Second International Symposium on the Utilization of High Strength Concrete was held in Berkeley, CA, May 1990. A substantial amount of research work and project construction with high strength concrete was completed since the last Symposium. Recent findings were presented and discussed.