Title: SP-013: Symposium on Reinforced Concrete Columns

Author(s): Editor: Boris Bresler

Publication: Symposium Paper

Volume: 13

Issue:

Appears on pages(s): 378

Keywords:

DOI: 10.14359/14065

Date: 1/1/1966

Abstract:
SP13 Selected papers dealing with experimental and analytical studies of reinforced and prestressed concrete columns, are contained in this volume. Compilation of the papers has been carried out under the sponsorship of the joint ACI-ASCE Committee 441, Reinforced Concrete Columns, in accordance with the committee’s three main objectives: (I) to review and correlate information on the analysis and design of concrete columns, including the methods required by various building codes; (2) to encourage experimental research on column behavior; (3) to propose design criteria for concrete columns.