Title: SP-081: Fiber Reinforced Concrete--International Symposium

Author(s): Editor: George C. Hoff

Publication: Symposium Paper

Volume: 81

Issue:

Appears on pages(s): 460

Keywords:

DOI: 10.14359/14038

Date: 11/1/1984

Abstract:
SP81 The nineteen papers in this volume are divided into three parts. Part I deals with structural application and design and previous information on the use of fiber reinforced concrete in structural elements. Part II deals with applications, materials, and techniques for evaluating fiber reinforced concrete. Part III consists of committee reports on: A) state-of-the-art report on fiber reinforced concrete; B) measurement of properties of fiber reinforced concrete; C) guide for specifying, mixing, placing, and finishing steel fiber reinforced concrete.