SP-213: The Art and Science of Structural Concrete Design

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: SP-213: The Art and Science of Structural Concrete Design

Author(s): Editor: S. Ali Mirza

Publication: Symposium Paper

Volume: 213

Issue:

Appears on pages(s): 246

Keywords:

DOI: 10.14359/14023

Date: 5/22/2003

Abstract:
This Symposium Publication is a compilation of 13 papers presented at a sympsoium held at the 2002 ACI Spring Convention in Detroit honoring Richard W. Furlong. Topics include high-strength high-performance concrete columns and biaxial bending, the rold of FRP reinforcement and strut-and-tie models, the use of precast prestressed concrete in building and highway pavements, composite steel-concrete construction, and the teaching of structural concrete design. Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP213