Title: SP-207: Proceedings, 3rd Intl Conf on High Performance Concrete: Performance and Quality of Concrete Struct

Author(s): Editors: V.M. Malhotra, Paulo Helene, Enio P. Figuerido, and Armando Carniero

Publication: Symposium Paper

Volume: 207

Issue:

Appears on pages(s): 514

Keywords:

DOI: 10.14359/14016

Date: 10/7/2002

Abstract:
This Symposium Publication includes 30 papers selected from the Third Conference on High-Performance Concrete (HPC) and Performance and Quality of Concrete Structures, held in Brazil. Topics covered include chloride penetration models in reinforced concrete structures, high-strength concrete with crushed and natural sand, sewage sludge ash as an addition in concrete, and the mechanical properties of polymer-modified high-performance lighweight aggregate concrete. Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP207