SP-199: Seventh CANMET/ACI Intl Conf on Fly Ash, Silica Fume, Slag and Natural Pozzolans in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: SP-199: Seventh CANMET/ACI Intl Conf on Fly Ash, Silica Fume, Slag and Natural Pozzolans in Concrete

Author(s): V.M. Malhotra

Publication: Symposium Paper

Volume: 199

Issue:

Appears on pages(s): 957

Keywords:

DOI: 10.14359/14006

Date: 6/1/2001

Abstract:
Conditioning coal-burning power-plant flue gases with ammonia reduces the emission of nitrous oxide compounds. But the ammonia often combines with available sulfur and other compounds that attach to the fly ash. If the ammoniated fly ash is then used in concrete, the high-pH environment causes a release of ammonia and a strong, objectionable ammonia smell. This can make the fly ash unmarketable. What’s the solution? Fly ash beneficiation processes that can remove ammonia and also reduce the unburned carbon content. Some of the processes are described in one of the 54 papers included in ACI SP-199, Seventh CANMET/ACI International Conference on Fly Ash, Silica Fume, Slag and Natural Pozzolans in Concrete. Other papers deal with effects of fly ash and admixture combinations on setting time, use of slag concrete to reduce corrosion of reinforcement, and the role of chemical and mineral admixtures in concrete made with recycled concrete as aggregate. Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP199