Design of Concrete Members Subjected to Uniaxial Bending and Compression Using Reinforcement Sizing Diagrams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design of Concrete Members Subjected to Uniaxial Bending and Compression Using Reinforcement Sizing Diagrams

Author(s): Enrique Hernandez-Montes, Luisa Maria Gil-Martin, and Mark Aschheim

Publication: Structural Journal

Volume: 102

Issue: 1

Appears on pages(s): 150-158

Keywords: beams; columns; prestressed concrete; reinforced concrete

DOI: 10.14359/13540

Date: 1/1/2005

Abstract:
Traditional approaches to the design of reinforced concrete members for flexural moment and axial load have emphasized analysis to determine the location of the neutral axis for a given configuration of longitudinal reinforcement and axial load. An alternate approach is described in this paper, wherein the reinforcement required to resist the specified design moment and axial load is determined as a function of the neutral axis depth. A range of neutral axis depths is considered, resulting in a number of potential design solutions consisting of different combinations of top and bottom reinforcement. These potential design solutions are portrayed graphically using a new diagram termed a reinforcement sizing diagram (RSD). The comprehensive set of solutions displayed by the RSD provides a basis for the design engineer to select a specific combination of top and bottom reinforcement to be used in a particular design. Reinforcement may be selected to minimize total reinforcement area or to accommodate nominal amounts of compression reinforcement as may be required for convenience in construction. Several examples are presented, illustrating the technique according to the assumptions adopted in the provisions of ACI 318 and Eurocode 2. The effects of optimal reinforcement on the axial load-moment interaction diagram are illustrated for one example.