Ductile FRP Strengthening Systems

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ductile FRP Strengthening Systems

Author(s): Nabil F. Grace, Wael F. Ragheb, and George Abdel-Sayed

Publication: Concrete International

Volume: 27

Issue: 1

Appears on pages(s): 31-36

Keywords: Rehabilitation; external strengthening; repair; epoxy bond; fiber reinforced polymer

DOI:

Date: 1/1/2005

Abstract:
Fiber-reinforced polymer (FRP) products have become attractive materials for structural engineers in the concrete construction field, especially for strengthening existing reinforced concrete structural elements. Unfortunately, there are several drawbacks associated with using commercially available FRP systems for flexural and/or shear strengthening of reinforced concrete beams. The objective of this article is to introduce two hybrid, pseudo-ductile FRP strengthening systems designed to potentially avoid many of these drawbacks.