Avoiding the Rehabilitation of Cooling Towers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Avoiding the Rehabilitation of Cooling Towers

Author(s): Leandro Etcheverry

Publication: Concrete International

Volume: 27

Issue: 1

Appears on pages(s): 27-30

Keywords: cooling tower; repair; cathodic protection; water distribution; reinforcement corrosion

DOI:

Date: 1/1/2005

Abstract:
Natural draft hyperbolic cooling towers are extremely conducive to corrosion-induced deterioration. By understanding the deterioration mechanisms and the effective rehabilitation strategies, however, the life and value of natural-draft hyperbolic cooling towers can be maximized. A variety of state-of-the-art concrete repair technologies, augmented with high-performance construction materials and protection systems, are available to implement cost-effective repair programs.