350.2R-04: Concrete Structures for Containment of Hazardous Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 350.2R-04: Concrete Structures for Containment of Hazardous Materials

Author(s): ACI Committee 350

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 17

Keywords: construction joint; joint; joint sealant; precast concrete; prestress; water-cementitious material ratio; waterstop.

DOI:

Date: 6/28/2004

Abstract:
This report presents recommendations for structural design, materials, and construction of structures commonly used for hazardous materials containment, including reinforced concrete tanks, sumps, and other structures that require dense, impermeable concrete with high resistance to chemical attack. The report discusses and describes design and spacing of joints, proportioning of concrete, placement, curing, and protection against chemicals. Information on liners, secondary containment systems, and leak- detection systems is also included.