440.4R-04: Prestressing Concrete Structures with FRP Tendons

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 440.4R-04: Prestressing Concrete Structures with FRP Tendons

Author(s): ACI Committee 440

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 35

Keywords: anchorage; bond length; crack; deflection; deformation; development length; ductility; fatigue; jacking stresses; post-tensioning; prestressed concrete; pretensioning; reinforcement ratio; shear; tendon.

DOI:

Date: 9/21/2004

Abstract:
Fiber-reinforced polymers (FRPs) have been proposed for use instead of steel prestressing tendons in concrete structures. The promise of FRP materials lies in their high-strength, lightweight, noncorrosive, nonconducting, and nonmagnetic properties. This document offers general information on the history and use of FRP for prestressing applications and a description of the material properties of FRP. The document focuses on the current state of design, development, and research needed to characterize and ensure the performance of FRP as prestressing reinforcement in concrete structures. The proposed guidelines are based on the knowledge gained from worldwide experimental research, analytical work, and field applications of FRPs used as prestressed reinforcement. The current development includes a basic understanding of flexure and axial prestressed members, FRP shear reinforcement, bond of FRP tendons, and unbonded or external FRP tendons for prestressing applications. The document concludes with a description of research needs.