Span-by-Span Bridge Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Span-by-Span Bridge Construction

Author(s): Boris Levintov, Kenneth V. Butler, and Randy Hart

Publication: Concrete International

Volume: 26

Issue: 12

Appears on pages(s): 46-50

Keywords: segmental bridge; concrete box girder; median; construction equipment

DOI:

Date: 12/1/2004

Abstract:
The Tampa-Hillsborough County Expressway is an elevated, reversible-lane highway that eases traffic congestion for commuters between the cities of Tampa and Brandon, FL. Included in the project are two, at-grade roadway sections and three, segmental concrete box girder bridges. This article describes the challenges faced by engineers during design of construction equipment for the bridges.