Title: Concrete, Construction, or Salt—Which Causes Scaling? Part 2

Author(s): Dipayan Jana

Publication: Concrete International

Volume: 26

Issue: 12

Appears on pages(s): 51-56

Keywords: finishing; air-void systems; loss of air; excess water

DOI:

Date: 12/1/2004

Abstract:
This second part describes three case studies where, despite having good air-void systems, the concrete scaled. It is theorized that the concrete scaled due to improper finishing practices such as: a) initiation of finishing prior to the cessation of bleeding (entrapping bleed water under the finished surface); b) finishing in the presence of excess water at the surface, which reduces the scaling and abrasion resistance of the surface; and c) prolonged finishing, which severely reduces the air content at the surface and increased the concrete’s potential to scale.