Concrete, Construction, or Salt—Which Causes Scaling?

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete, Construction, or Salt—Which Causes Scaling?

Author(s): Dipayan Jana

Publication: Concrete International

Volume: 26

Issue: 11

Appears on pages(s): 31-38

Keywords:

DOI:

Date: 11/1/2004

Abstract:
Part I of this article provides three case studies that demonstrate the roles of lack of air entrainment, improper air entrainment (coarse air void system), and inadequate air entrainment (low entrained air content) in scaling. Part II will provide three case studies to show scaling due to initiation of finishing prior to the cessation of bleeding, finishing in the presence of excess water at the surface, and prolonged finishing practices. A poor air-void system causes scaling of the concrete surface at saturated conditions during cyclic freezing and thawing. Finishing improprieties, on the other hand, can cause scaling, abrasion, or delamination even in the absence of cyclic freezing and thawing