Cementitious Adhesive for Ceramic Tiles

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cementitious Adhesive for Ceramic Tiles

Author(s): Arvind K. Suryavanshi

Publication: Concrete International

Volume: 26

Issue: 8

Appears on pages(s): 63-68

Keywords: Proportioning; single-pack; durability; polymer; bond

DOI:

Date: 8/1/2004

Abstract:
Contemporary cementitious tile adhesives are available either as single-pack systems or two-pack systems. By judicious selection and proportioning of cement, filler, polymer, water-retention agent, and auxiliary chemicals, it is possible to formulate a single-pack tile adhesive having superior engineering and durability properties. The present article describes the engineering and durability properties of a single-pack tile adhesive formulated by the author.