Title: 351.3R-04: Foundations for Dynamic Equipment

Author(s): ACI Committee 351

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 63

Keywords: amplitude; concrete; foundation; reinforcement; vibration.

DOI:

Date: 5/3/2004

Abstract:

Note: A newer version of this document exists. This document was replaced by 351.3R-18.

This report presents to industry practitioners the various design criteria and methods and procedures of analysis, design, and construction applied to dynamic equipment foundations.