Lunar Concrete Update

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Lunar Concrete Update

Author(s): T. D. Lin and Nan Su

Publication: Concrete International

Volume: 13

Issue: 11

Appears on pages(s): 73-76

Keywords: concrete construction; lunar bases; lunar structures; temperature; structural design; tests; General

DOI:

Date: 11/1/1991

Abstract:
NASA provided Construction Technology Laboratories, Inc. with lunar soil samples in 1986 and funds in subsequent years to experimentally investigate the feasibility of using concrete for lunar construction. The test programs include studies on the physical properties of concrete made with lunar soil, lunar cement production, preliminary designs of concrete lunar habitats, and the effects of lunar temperatures upon concrete.