Title: Santee Cooper Shotcrete Repair in Moncks Corner

Author(s): W. L. Snow

Publication: Concrete International

Volume: 13

Issue: 11

Appears on pages(s): 28-31

Keywords: architectural concrete; concrete construction; office buildings; repairs; shotcrete; General

DOI:

Date: 11/1/1991

Abstract:
Santee Cooper, a major electrical supplier in Moncks Corner, South Carolina, entered a contract to construct a three-story annex. Construction was halted due to apparent deviation for the original architecture and remedial action had to be taken. Shotcrete was settled on as the repair method.