Corrosion Study of Stainless Steel Bars in Cracked Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Corrosion Study of Stainless Steel Bars in Cracked Concrete

Author(s): T. Yamaji, T. Hirasaki, R. Takahashi, S. Mizuma, and M. Yamakawa

Publication: Symposium Paper

Volume: 222

Issue:

Appears on pages(s): 155-170

Keywords: chloride; corrosion; cracked concrete; stainless steel

DOI: 10.14359/13311

Date: 5/1/2004

Abstract:
Corrosion of stainless steel bars in concrete was investigated using sound and pre-cracked concrete specimens. Three types of stainless steel were investigated, such as 18Cr, 18Cr-8Ni and 18Cr-12Ni-2.5Mo. Concrete specimens were exposed to two environments, where wetting and drying alternately repeated. One was in the outdoor with atmospheric temperature, and the other was in a controlled chamber, where the temperature was 60°C during wetting and 15°C during drying. The detail investigation was carried out after two years. No corrosion was observed on stainless steel bar in both sound and pre-cracked concrete exposed to outdoor. The maximum chloride ion concentration was 7.0 kg/m3 for 18Cr-8Ni, 8.0 kg/m3 for 18Cr-12Ni-2.5Mo and 6.0 kg/m3 for 18Cr at the crack region of concrete. This result indicated that the chloride ion threshold level for stainless steel was larger than these values under marine environment with atmospheric temperature. No corrosion was observed on both 18Cr-12M-2.Wo and 18Cr in both sound and pre-cracked concrete exposed to controlled chamber. However, corrosion was observed only for 18Cr-8Ni at the crack region, even when the chloride ion concentration at the crack region was 6.0 kg/m3. This was considered to be due to the effect of a high temperature.