Influence of Blast Furnace Slag on Durability of High-Strength Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Blast Furnace Slag on Durability of High-Strength Concrete

Author(s): Y. Sagawa, H. Matsushita, Y. Maeda, I Chikada, and S. Kaneyasu

Publication: Symposium Paper

Volume: 221

Issue:

Appears on pages(s): 703-720

Keywords: carbonation; chloride; deicing salts; ground granulated blast-furnace slag; high strength concrete; prestressed concrete; salt attack

DOI: 10.14359/13286

Date: 5/1/2004

Abstract:
Although the water-cement ratio of concrete for the prestressed concrete is low, deterioration due to salt attack of prestressed concrete structures has appeared in recent years. Blast-furnace slag is effective in resisting penetration of chloride ions. However, the influences of blast-furnace slag on the durability properties of high-strength concrete for steam-cured pretensioned elements are not clear. In this study, carbonation and chloride penetration of the high-strength concrete using blast-furnace slag were examined. As the result, the addition of blast-fumace slag increased the concentration of chloride ion near the surface, but decreased the penetration to the interior concrete. Blast-furnace slag improved the resistance to erosion by a calcium chloride solution. Moreover, it was found that carbonation of the concrete made with blast-furnace slag was slow and there was no problem in this respect.