Properties of Flowable Self-Compacting Slurry Using Quarry By-Products and Ponded CCPs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Properties of Flowable Self-Compacting Slurry Using Quarry By-Products and Ponded CCPs

Author(s): I R. Naik, R. N. Kraus, Y. Chun, R. Siddique, and E D. Botha

Publication: Symposium Paper

Volume: 221

Issue:

Appears on pages(s): 523-538

Keywords: compressive strength; fine crushed sand; flowable slurry; ponded CCP; quarry by-products; settlement; water permeability

DOI: 10.14359/13275

Date: 5/1/2004

Abstract:
This paper reports the properties of two series of flowable self-compacting slurry. In Series 1, five mixtures of flowable slurry were made using ponded coal-combustion fly ash and quarry screenings (fine crushed sand). In Series 2, six mixtures of flowable slurry were made, the first five mixtures using the ponded coal-ash and natural sand, and the final one mixture using Class C fly ash and natural sand. Ash and quarry-screenings contents of the mixtures are expressed as percentages of the sum of the quantities of the ash and aggregate. For Series 1 flowable-slurry mixtures, ponded-ash content was 100, 67, 53, 35, and 0 percent, and quarry-screenings content was 0, 33, 47, 65, and 100 per-cent, respectively. In Series 2 flowable-slurry mixtures, ash content was 100, 81, 60, 40, 20, and 4 percent, and sand content was 0, 19, 40, 60, 80, and 96 percent, respectively. For both series of flowable-slurry mixtures, tests were performed for flow, density, settlement, compressive strength, and permeability. Ambient air and slurry temperatures were also recorded. Compressive strength of both Series 1 and Series 2 mixtures increased with age. Compressive strength of Series I mixture was higher than Series 2 mixtures. It was also observed that the permeability of flowable-slurry mixtures decreased with increase in age due to improvement in microstructure and increase in strength of the flowable-slurry mixtures. Mixtures containing quarry screenings were also less permeable.