The Influence of Slag and Fly Ash on the Carbonation of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Influence of Slag and Fly Ash on the Carbonation of Concrete

Author(s): M. Collepardi, S. Collepardi, J. J. Ogoumah Olagot, and E Simonelli

Publication: Symposium Paper

Volume: 221

Issue:

Appears on pages(s): 483-494

Keywords: carbonation; compressive strength; fly ash; ground limestone; mineral addition

DOI: 10.14359/13272

Date: 5/1/2004

Abstract:
The paper shows the influence of mineral additions (in form of fly ash, slag and ground limestone) replacing portland cement on the COz penetration rate of concretes manufactured at a given water-cementitious material ratio (w/cm). The results indicate that at a given w/cm there is an increase in the carbonation rate in concretes with mineral additions, except when the amount of portland cement replacement is relatively low (15%). On the other hand, when the comparison of the carbonation rate is made on concretes at the same strength level, there is no significant difference between concretes with portland cement and those with replacement by mineral addition up to 50%.