Title: CP-29(02)A: Concrete Strength Testing Video

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 1/1/2002

Abstract:
Four ASTM Standards are covered on this video: C39, C78, C617, and C1231. This video may be used to supplement training in preparation to take theACI Concrete Strength Testing Technician examinations


Product unavailable, please call +1.248.848.3800