CP-14(85)A: Laboratory Testing -- Tape #3

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: CP-14(85)A: Laboratory Testing -- Tape #3

Author(s): ACI Committee E902 and Portland Cement Association

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/1/1986

Abstract:
Three ASTM Standard Test Methods on aggregate are demonstrated. The ASTM tests covered are: C78-Flexural Strength of Concrete C123-Lightweight Pieces in Aggregate C192-Making and Curing Concrete Test Specimens in the Laboratory